MIL-DTL-50647B
4.6.5 Box, Packing, Ammunition, Drawing 8799620.
Characteristic
Defect
Method of Inspection
Critical
None defined
Major
None defined
Minor
201
Contents loose
Manual/Visual
202
Strapping missing, loose, broken, or improperly assembled
Visual
203
Contents of box exposed
Visual
204
Box damaged
Visual
205
Marking missing, incorrect, or illegible
Visual
206
Number of cartons incorrect
Visual
4.6.6 Carton, Alternative, Packing, Drawing 9224944.
Characteristic
Defect
Method of Inspection
Critical
None defined
Major
None defined
Minor
201
Contents loose
Manual
202
Box broken or damaged
Visual
203
Number of units contained incorrect
Visual
204
Marking missing, incorrect, or illegible
Visual
205
Tape incomplete
Visual
4.7 Test methods and procedures.
4.7.1 Ignition device x-ray. Prior to assembly into the cartridge, the ignition device shall be
radiographically examined in accordance with ASTM E1742. Each ignition device shall be x-rayed on
boards or trays with the cup side perpendicular to the rays. The x-ray negatives shall be identified by
item nomenclature and by lot number. Ignition devices are to be left mounted to the boards or trays until
after the x-rays have been reviewed and defects identified to facilitate removal of defective units. After
screening, the x-ray negatives with defectives identified, shall be forwarded to the engineering activity
designated by the acquiring activity. Interpretation of the radiographic films shall verify the following:
missing or abnormally thin charge; charge broken, cracked, or porous; cracked or off-center anvil or other