MIL-C-45408C
Characteristic
Defect
Method of Inspection
Critical
1
Improper assembly
Visual/X-ray
2
Any part missing
Visual/X-ray
3
Primer pellet broken, cracked, or dislodged
Visual
4
Metal defective
Visual
5
Primer foil discolored
Visual
6
Mixed primers
Visual
Major
101
Burr
Visual
102
Foreign matter present
Visual
4.6.3 Case, Cartridge, Drawing 8594158, covering a detail of Drawing 8593276.
Critical
1
Metal defective
Visual
Major
101
Concentricity of large diameter with small diameter
Gage
102
Diameter of head, min
Gage
103
Thickness of base, min
Gage
104
Diameter of body, min
Gage
105
Thickness of sidewall, min
Gage
106
Straightness of base
Gage
107
Protective finish inadequate or defective
Visual
108
Foreign matter present
Visual
109
Burr or sharp corner
Visual
Minor
201
Small diameter, max
Gage
202
Large diameter, max
Gage
203
Total length
Gage
204
Location of datum diameter
Gage
205
Thickness of sidewall, max
Gage
206
Radius or chamfer missing or incorrect, except as otherwise
classified
Visual
207
Surface finish improper
Visual
4.6.4 Head, Cartridge, Drawing 8594159, covering a detail of Drawing 8593276.
8